AFNOR X2CrNiMo17-12-2
The high quality France AFNOR X2CrNiMo17-12-2 material is one of the more steel grades we supply, Austenite.
X2CrNiMo17-12-2 is our main production grade, which has been approved by customers in many countries since its initial production, including our X2CrNiMo17-12-2 round bars, flat bar, forgings, fasteners, tubes, wires, strips, sheets & Plates, as well as a variety of profiles, professional high precision auto-lathe processing manufacturer of clinching fasteners, axes, standoffs, screws, studs, nuts, bolt, OEM parts and special shaped turning partsthe state of delivery includes quenched and tempered, annealed, machined semi-finished products, we also have strict management of the packaging, to avoid material damage from transportation. We are the best supplier of X2CrNiMo17-12-2 materials, and we are willing to develop together with customers from all over the world.
Also includes X2CrNiMo17-12-2 steel material norm, chemical composition, mechanical
properties, datasheet, X2CrNiMo17-12-2 equivalent, heat treatment and temperature process of X2CrNiMo17-12-2, The peak hardness can be achieved, Contains all of the specification, welding properties, let us in X2CrNiMo17-12-2 this steel grade have a more comprehensive understanding, Download the full X2CrNiMo17-12-2 PDF version of this datasheet.
2015-08-10 15:52:10
Print this page
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) |
Max 0.030 | Max 1.00 | Max 2.00 | Max 0.045 | Max 0.015 | 16.50-18.50 | 10.00-13.00 | 2.00-2.50 |
N(%) |
Max 0.11 |
Rp0.2 (MPa) |
Rm (MPa) |
Impact KV (J) |
Elongation A (%) |
A Z (%) |
Delivery |
Hardness HB |
522 (≥) |
861 (≥) |
32 |
33 |
34 |
Solution & Aging, Ann, Ausaging, Q+T |
433 |