UNS NO7718 Inconel 718 2 4668 Round bar

Product Details

Item Element Min Max Similar Note
1 Ti 0.6000 1.2000 -  
2 Si - 0.3500 -  
3 S - 0.0150 -  
4 P - 0.0150 -  
5 Ni 50.0000 55.0000 -  
6 Nb+Ta 4.7000 5.5000 -  
7 Mo 2.8000 3.3000 -  
8 Mn - 0.3500 -  
9 Fe - - - Remainder
10 Cu - 0.3000 -  
11 Cr 17.0000 21.0000 -  
12 Co - 1.0000 -  
13 C 0.0200 0.0800 -  
14 B 0.0020 0.0060 -  
15 Al 0.3000 0.7000 -