Nimonic 80A | NiCr20TiAl|2.4952|UNS N07080|BS 3HR1 Forging Bars

Nimonic 80A | NiCr20TiAl|2.4952|UNS N07080|BS 3HR1 Forging Bars

Nimonic 80A | NiCr20TiAl|2.4952|UNS N07080|BS 3HR1 Forging Bars
$ 1,000.00 In stock
  • Name: Nimonic 80A | NiCr20TiAl|2.4952|UNS N07080|BS 3HR1 Forging Bars
  • Standard: ASTM
  • Surface: Turned 、
  • Status: Hot-Rolled 、Solutioned 、
  • Stock: Order
  • Tags: 80A, Nimonic, NiCr20TiAl, 2-4952, N07080, 3HR1,

Quick Details

GE spec NB 00146, Ideally released to GE spec NB 00146 or to ASTM B637 or WK 2 4952 or BS 3HR1, VIM+ESR, Hot Forging,Polishing,

Product Details

GE spec NB 00146, Ideally released to GE spec NB 00146 or  to ASTM B637 or WK 2.4952 or BS 3HR1, VIM+ESR, Hot Forging,Polishing,

Grade

2.4952

Nimonic 80A

C

0.04~0.10

0.10

Si

1.00

1.00

Mn

1.00

1.00

P

0.020

S

0.015

0.015

Ni

65.00

Balance

Cr

18.00~21.00

18.00~21.00

Ti

1.80~2.70

1.80~2.70

Al

1.00~1.80

1.00~1.80

Co

1.00

2.00

Fe

1.50

3.00

Cu

0.20

0.20

B

0.008

0.008

Zr

0.15

Pb

0.0025